WARNINGSpecifications
Made In
US
Weight
0.75lb
Applicable Materials
Metals
Brand
Sprayon
Capacity Vol. [Nom]
9 oz
Category
Penetrants
Packing Type
Aerosol Can
Physical Form
Liquid
Temp. Range [Max]
122 °F
Type
Developer
Viscosity @ Temp. [Nom]
20.5 cSt @ 104°F
Wt.